X-ray fluorescence (XRF) spectroscopy is a powerful technique for both process control and regulatory compliance in the polymers and plastics industry . Reliable monitoring of the concentration of remaining catalysts helps to accurately control the polymerization process and ensures the maximum allowable concentration for several restricted elements is not exceeded.
XRF delivers important advantages compared to other elemental analysis techniques. Sample preparation is straightforward, with no dissolution required. Measurements are non-destructive and results are accurate and reproducible. Time-consuming and costly re-standardizations are unnecessary and the resultant data are consistent over long periods, saving time and money. Automated analysis reduces measurement times to a matter of minutes and efficient sample preparation methods support high throughput. User-friendly software allows routine analysis to be carried out by factory operators.
Expertise program for XRF analysis of toxic elements in polymers and plastics
This Expertise program delivers a complete methodology from sample preparation to quality assurance for elemental analysis in polyolefins (all kinds of PP and PE, including iPP, HDPE, LDPE, mPE, ULMWPE etc.). It can be applied to Zetium, Axios, MagiX or Epsilon range systems. The following elements and concentration ranges are covered:
Elements | ppm |
Cr | 0 - 22 |
Ni | 0 - 11 |
Cu | 0 - 25 |
Zn | 0 - 5 |
As | 0 - 6 |
Br | 0 - 160 |
Cd | 0 - 30 |
Ba | 0 - 600 |
Hg | 0 - 5 |
Pb | 0 - 22 |