The appearance of wear metals in lubricating oils is a significant indicator of component wear or contamination. Accurate XRF analysis of trace elements in oil, and monitoring their levels over time, helps optimize preventive maintenance programs. The data can be used for an early detection of potentially expensive failures, this way reducing repair costs and increasing safety margins.
Expertise program for XRF analysis of wear metals in lubrication oils
The following elements and concentration ranges are covered by the Wear Metals Expertise program:
Elements | ppm | Elements | ppm |
Ag | 0 - 500 | Mo | 0 - 500 |
Al | 0 - 2000 | Na | 0 - 500 |
Ba | 0 - 2000 | Ni | 0 - 500 |
Ca | 0 - 5000 | P | 0 - 2000 |
Cd | 0 - 500 | Pb | 0 - 500 |
Cr | 0 - 500 | Sb | 0 - 500 |
Cu | 0 - 400 | S | 0 - 500 |
Fe | 0 - 500 | Sn | 0 - 500 |
K | 0 - 500 | Ti | 0 - 500 |
Mg | 0 - 3000 | V | 0 - 500 |
Mn | 0 - 500 | Zn | 0 - 2000 |
In addition to standards, the program includes a complete methodology, from sample preparation to quality assurance, to be used with Malvern Panalytical’s XRF systems.
Included:
Optional
Prerequisites
Contact our specialists
* SPC is already included with Zetium systems