Stabilising slurries: Understanding the influence of concentration on the zeta potential measurement of TiO2 slurries

The maximum sample concentration at which zeta potential measurements can be made is limited by the cell path length. A high concentration cell option for the Zetasizer Nano increases the maximum concentration