Smart VacPrep

The Micromeritics Smart VacPrep is an advanced six-port system that utilizes a vacuum to prepare samples by heating and evacuation.

索取報價 要求演示 聯繫銷售部門

Overview

The Smart VacPrep is an advanced six-port system that utilizes vacuum to prepare samples by heating and evacuation. Each of the ports may be operated independently. 

Samples may be added or removed from degas ports without disturbing the treatment of other samples undergoing preparation. Degassing automatically terminates when the samples have completed all programmed steps.

規格

能力样品处理量
Six ports
Degas
Heat and vacuum
Vacuum control Servo-controlled rates to minimize or eliminate sample elutriation
Evacuation rate Selectable evacuation rate from 1.0 to 50.0 mmHg/s
样品加热
Heating mantles
温度范围
40 to 450 ºC in one degree increments
温度控制范围
One ramp during evacuation phase, five additional ramps during subsequent phases
温度精确性
Deviation less than ±10 ºC at the sensing thermocouple embedded in the heating mantle
Heating ramp rate
Selectable from 0.1 ºC per minute to 10 ºC per minute
Hold time
Zero to 999 minutes in one-minute increments
Backfill options
Automatic backfill
尺寸:
Height 69 cm (27 in.), Width 53 cm (21 in.), Depth 43 cm (17 in.)
重量
70 lbs (32 kg)