FlowPrep

The Micromeritics FlowPrep lets you choose the most suitable gas, temperature, and flow rate for your application and sample material.

索取報價 要求演示 聯繫銷售部門

Overview

The Micromeritics FlowPrep applies a combination of heat and a stream of inert gas to your sample. The heat causes contaminants to desorb from the surface, and the stream of inert gas sweeps them out of the sample tube. 

The FlowPrep lets you choose the temperature, gas, and flow rate best suited for your sample material and application. 

Needle valves allow you to introduce the flowing gas slowly to prevent fluidization of samples.

規格

Sample tubes Up to 3.0-cm (1.18-in.) OD
Heating block
Temperature: 10 ºC above ambient to 400 ºC
Temperature Accuracy: ± 10 ºC
電功率
Voltage: 100, 120, 220, 240 VAC ± 10%
Power: 250 VA maximum
Frequency: 50/60 Hz
Environment
Temperature: 10 to 35 ºC operating; 0 to50 ºC non-operating
Humidity: 45 to 80% relative, non-condensing
Gas Consumption
Helium, nitrogen, argon, or any other pure gas that does not adsorb at room temperature
流速范围 Up to 50 cm3/min. No vacuum required
样品容量
6 heating stations and 6 cooling stations
尺寸:
Height: 45 cm (16.93 in.)
Width: 36 cm (14.17 in.)
Depth: 30 cm (11.81 in.)