Overview
The Micromeritics FlowPrep applies a combination of heat and a stream of inert gas to your sample. The heat causes contaminants to desorb from the surface, and the stream of inert gas sweeps them out of the sample tube.
The FlowPrep lets you choose the temperature, gas, and flow rate best suited for your sample material and application.
Needle valves allow you to introduce the flowing gas slowly to prevent fluidization of samples.
사양
Sample tubes | Up to 3.0-cm (1.18-in.) OD |
---|---|
Heating block | Temperature: 10 ºC above ambient to 400 ºC
Temperature Accuracy: ± 10 ºC |
전원 | Voltage: 100, 120, 220, 240 VAC ± 10%
Power: 250 VA maximum
Frequency: 50/60 Hz |
Environment | Temperature: 10 to 35 ºC operating; 0 to50 ºC non-operating
Humidity: 45 to 80% relative, non-condensing |
Gas Consumption | Helium, nitrogen, argon, or any other pure gas that does not adsorb at room temperature |
흐름 속도 범위 | Up to 50 cm3/min. No vacuum required |
샘플 용량 | 6 heating stations and 6 cooling stations |
크기 | Height: 45 cm (16.93 in.)
Width: 36 cm (14.17 in.)
Depth: 30 cm (11.81 in.)
Weight: 8.6 kg (19 lbs) |