00:00:00 | Basic theory of automated particle imaging? |
00:00:22 | Basics Principles of Automated particle Imaging |
00:01:11 | Sample Dispersion |
00:02:11 | Image Capture and Analysis |
00:02:54 | Morphological shape descriptors |
00:04:08 | The third dimension - gives extra information |
00:04:46 | Number – Volume Relationship |
00:05:32 | Number distribution |
00:05:58 | Volume distribution |
00:06:33 | Minimum number of pixels |
00:07:43 | Summary – Basic Theory |
00:08:27 | Thank You |
This short presentation is designed to give you a brief introduction to automated particle imaging. Here, we discuss how automated imaging is carried out and some of the experimental and theoretical considerations that need to be taken into account.