ASTM C114-13 and ISO 29581-2 compliance for cement fused beads

With the latest innovations in X-ray tube and detector technology in the Epsilon 3XLE, this system, in combination with the Eagon 2 fully automatic fusion system, complies with the latest cement testing methods of both ASTM C114-13 and ISO 29581-2.

The data presented in this datasheet clearly demonstrate the compliance of the Epsilon 3XLE XRF spectrometer, in combination with the Eagon 2 automatic fusion machine, with both the ASTM C114- 13and ISO 29581-2:2010 cement test methods for the quantitative analysis of SiO2, Al2O3, Fe2O3, CaO, MgO, SO3, K2O, Na2O, TiO2, P2O5, ZnO and Mn2O3 in cement, prepared as fused beads. 