Analysis of raw mix samples prepared as pressed powders

This application note shows that the Epsilon 3X is capable of analyzing major and minor compounds like Na2O, MgO, Al2O3, SiO2, SO3, K2O, CaO, TiO2 and Fe2O3 in rawmix samples prepared as pressed powders.

In cement industry the composition of the input material plays a very important role in the production process and in the quality of the end product. XRF analysis is a useful tool of controlling the composition of the raw material. 