PE & PP types identification by FingerPrint

This application note demonstrates the capability of the FingerPrint application for distinguishing and recognizing several different PE and PP types and grades.

Different polyolefin types and grades, like mLLDPE, LLDPE, random PP and others, are not easily distinguishable with the naked eye. Measurements were performed using a PANalytical Epsilon 3XLE EDXRF spectrometer.