Investigating polymer degradation with triple detection GPC/SEC

Ultra high molecular weight PMMA was successfully analysed using advanced triple detection GPC. Gamma-sterilized PMMA was shown to have a much lower molecular weight, clearly indicating that the radiation had a polymer cleaving action
Ultra high molecular weight PMMA was successfully analysed using advanced triple detection GPC. Gamma-sterilized PMMA was shown to have a much lower molecular weight, clearly indicating that the radiation had a polymer cleaving action