The analysis of wear metals and additives in lubricating oils

This application note shows that the Epsilon 3XLE is capable of analyzing Mg, Al, Si, P, K, Ca, Ti, V, Cr, Mn, Fe, Ni, Cu, Zn, Mo, Cd, Sn, Sb, Ba and Pb in lubricating oil.

XRF is a powerful tool for analysis of wear metals in oil. This technology produces fast, cost-effective, accurate and precise data with a minimum sample preparation. 