00:00:00 | Introduction to Fiber Parameters measured on the Morphologi G3 |
00:00:11 | Caliper Measurements of Fibers |
00:00:40 | Fiber Total Length |
00:01:15 | Fiber Width |
00:01:34 | Comparison of calliper and fiber measurements |
00:02:09 | Fiber elongation: |
00:02:40 | Fiber straightness: |
00:03:02 | Application example 1 |
00:03:18 | Example 1 - Results |
00:03:49 | Comparison of width (caliper) and fiber width |
00:04:19 | Comparison of elongation (caliper) and fiber elongation |
00:04:40 | Application Example 2 |
00:04:58 | Width distribution (Caliper) |
00:05:16 | Fiber Width distribution |
00:05:41 | Conclusions |
This short presentation gives an overview of new functionality to analze fiber parameters with the Morphologi G3 system.