Studying the effect of gamma sterilisation on intra-ocular lens materials.

Intra-octular lenses, usually made from medical grade PMMA, need to be sterilized before use. Samples of Gamma ray sterilised polymer were studied. Triple detector GPC showed that irradiation cleaved the polymer at the branching points