NanoSight NTA Concentration Measurement Upgrade

NanoSight instruments with upgraded concentration measurement have increased concentration measurement accuracy and repeatability. This provides improved measurement robustness and removes the influence of user settings. Data is shown here that illustrates the improvement in measurement quality.

Providing repeatable and reproducible concentration measurements of nanoparticles

Concentration Measurement upgraded NTA systems increase concentration measurement accuracy and repeatability improving measurement robustness and removing the influence of user settings. This is achieved through upgrading the Concentration Measurement of systems individually to reduce the influence of user selected capture and analysis settings and adopting a protocol to provide greater repeatability of measurements:

Parameter

Specification

Instrument

NS300; NS500 (all lasers) with syringe pump

Repeatabilitya

3%   (15% before upgrade)

Reproducibilityb

10% (44% before upgrade)

Dilution Linearity error

13%

Concentration Range

1x106 – 1x109 particles per mL

Software

NTA 3.1

aCoefficient of variation (CV), bMAPE (Mean Absolute Percentage Error)

Principles of improvement

The NTA concentration measurement uses a dual approach to improve both repeatability and reproducibility.

Reproducibility & Accuracy:

The upgrade uses a dynamic value for observation volume. This reflects changes in the volume of liquid that particles are imaged in during video capture and analysis. These changes can be caused by a number of sample properties or user settings which may impact the amount of laser light scattered. This may change the depth of the field of view and therefore the volume particles are counted in and will influence measured concentration. Some examples of how sample properties or user settings can influence observation volume are found in the table below.

Parameter

Process

Effect on observation volume

Particle refractive properties

Greater scattering power of particles

High refractive index material increase observation volume

Particle size

Greater scattering power of particles

Larger sized particles increases observation volume

Camera level

Sensitivity to light capture

Higher camera level increases observation volume

Concentration

Increased number of scattering points – more scattered laser light

High concentration increases observation volume

By incorporating this dynamic value for observation volume, concentration measurement accuracy has been shown to increase significantly whilst removing the influence of user settings (Figure 1). Through these improvements reproducibility of measurements has also increased (Figure 2).

Figure 1. Removing the influence of Camera level and detection threshold from concentration measurements
Fig1_TN150515NTAConcentrationUpgrade.jpg
Figure 2. Increased reproducibility during an inter-laboratory comparison measuring exosomes
Fig2_TN150515NTAConcentrationUpgrade.jpg

The NTA Concentration Measurement Upgrade has also been shown to improve the accuracy and precision of non-standard samples including exosomes and microvesicles (Figure 3). In this sample type example, different users typically selected camera level 14, 15 or 16. 

Figure 3: Exosome concentration data showing improved accuracy and precision after the NTA Concentration Measurement Upgrade at three different camera levels.
Fig3_TN150515NTAConcentrationUpgrade.jpg

Repeatability:

Additionally, a protocol for sample delivery and measurement has been developed which has contributed to improvements in measurement repeatability. This protocol incorporates developments in both software and hardware to provide repeatability values as low as 3 % (CV). Figure 4 identifies the improvements in repeatability seen by imaging particles under flow compared to static within the sample chamber.

Figure 4. Comparison of flow and static concentration measurements of the same sample (boxes represent 10 x 60 second video capture)
Fig4_TN150515NTAConcentrationUpgrade.jpg

These combined steps provide repeatability values as low as 3 % (CV). Measurements of dilution linearity can provide accurate results with an error as low as 13 % across a concentration range of 1x106 – 1x109 particles per mL (subject to particle size and refractive index).